Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Tensile and compressive strength of the Carbon Fibre Tape Plain Weave...
Tensile and compressive strength of the Carbon Fibre Tape Plain Weave 232g 25 mm
Post Reply
Like
5
Tensile and compressive strength of the Carbon Fibre Tape Plain Weave 232g 25 mm
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Rob Rav
Rob Rav
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 4
Hi,
I wondered if you can help I am underfed taking an Open University project on the amount of carbon fibre and epoxy needed to bind an Bamboo bike together. As such I need to know the material strength of the Carbon Fibre Tape Plain Weave 232g 25 mm that I bought off you, is it possible to supply these values when it is used with an epoxy??
Thank you,
Rob
Reply
Like
5
Warren (Staff)
Warren (Staff)
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Hi Rob,
We would not have exact data for a laminate of the tape and epoxy as every epoxy is different and there are so many different variables of construction and layup that would effect the final properties. You would be best simulating the effects through FEA on a CAD package to get some reasonably accurate results for your desired laminate.
However we can certainly give you the base properties of the materials. The resin specifications are found on each products listing and Technical Data Sheet. If you struggle to find these, I can email you the data for your chosen resin(s). In terms of the tape properties, our
Carbon Fibre Tape Plain Weave 232g
is made using Mitsubishi Rayon Pyrofil TR30S 3K fibres. The data sheet for the tape can be found here:
Carbon Fibre Tape TDS
and the data sheet for the fibre can be found here:
Mitsubishi Rayon Pyrofil TR30S 3K.
With both these datasheets you should be able to calculate some specific figures for your application.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search