I have been using Vac Cast for some time now, but I need to put a very good finish on a master before making the mould. Is it OK to spray it with 2k paint and then polish?? Some casting resins don't like paint.
I have also been using release film from you but would like to try the one with perforated version, slly question I know but where does the epoxy go if it comes out of the holes? Is it just into the bag.
Thanks for great products keep up the good work.

Mike
Mikes Racing Product
meir
meir
Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)
Group: Forum Members
Posts: 8, Visits: 117
Hi mike. 
I'm far from being an expert on that, but I think that on top of the release film you put this: