Finnluxury
Finnluxury
Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)
Group: Forum Members
Posts: 50, Visits: 448
I just released the Front mounting panel from the mould. All composites companies told me that its impossible part to be made. Too sharp edges and tight corners.. They told us to forget the idea of resin infusing this from carbon fiber. But we made it, and its perfect. We got a new nice solution to make it. Made with Easycomposites epoxy and carbon fiber.  Here is the video of it:

https://www.facebook.com/finnluxury/videos/1491915744152141/
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
That part looks stunning! Well done for the patience to get it right.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Finnluxury
Finnluxury
Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)
Group: Forum Members
Posts: 50, Visits: 448
Here is few new photos from our local show. The first photo with front end took me 10 minutes to attach over the chassis. Quite fast!  Our aim is to have all panels fitted to chassis less than 30 minutes.

http://www.talkcomposites.com/Uploads/Images/1b08c7c6-4cd8-4fa7-8bf1-551c.jpg


http://www.talkcomposites.com/Uploads/Images/dcd65109-96c5-49ef-9e44-fde6.jpg


http://www.talkcomposites.com/Uploads/Images/95bc1e91-8adb-499f-8442-160d.jpg
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
looking good
Finnluxury
Finnluxury
Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)
Group: Forum Members
Posts: 50, Visits: 448
Finnluxury
Finnluxury
Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)
Group: Forum Members
Posts: 50, Visits: 448
One new photo