Group: Forum Members
Posts: 3,
Visits: 16
|
Hello all,
I have finally got round to following up on this project. I have sanded down the polyester layer which turned cloudy, and bought the epoxy resin that was suggested as a topcoat. My polyester is now (naturally) matte, rather than shiny, because I have sanded it.
My question is: If I place the epoxy resin on top of the matte polyester, will my eventual finish be clear? Or will I still be able to see the matte polyester surface underneath the epoxy? If necessary, I can do another layer of polyester before the epoxy - so that the final polyester surface is shiny - but I would rather not if I can avoid it.
Many thanks to those who have taken the time to help with this.
|