Hi,
No need to do anything but add the epoxy on top! It will "fill in " the matte surface of the polyester - making the whole thing clear.
In essence, the "matte" surface on the polyester consists of a myriad of tiny scratches from the sanding, these will fill out with clear epoxy..
If you tried to polish the polyester, the epoxy will not bind to it, and would definitely delaminate very quickly..
Also remember to degrease the surface very thoroughly!!
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
|