Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Skinning advice
Skinning advice
Post Reply
Like
3
Skinning advice
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
MarkMK
MarkMK
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 338,
Visits: 2K
Not a technique I've had masses of experience with, but looking to do a little carbon skinning on some fairly small parts that have some subtle cosmetic features that I'd like to retain and not lose too much when adding material and coating
So, I was wondering if vacuum bagging the part once the fabric had been laid onto the tacky backing resin would help consolidate things a bit more tightly and help reduce the potential 'softening' of any subtle lines or features? I guess I'm asking if doing this will help to, in effect, de-bulk the single fabric layer and help make the skinned part a little closer to the original parts' dimensions and true form?
Just wondered if anyone regularly skinning parts did this or if it's unlikely to make any noticeable difference?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Skinning advice
MarkMK
-
10 Years Ago
I am wondering about the same thing. If vacuumbagging the part will help the carbon fiber to stick...
67redrocket
-
10 Years Ago
In theory, no, as the fabric itself should be dry and, assuming that it was laid down at the right...
MarkMK
-
10 Years Ago
It depends on the fine details that you are talking about. I've skinned parts with small grooves or...
Hanaldo
-
10 Years Ago
My wife and I usually try to vacuum bag using an extra food saver. What we do is, thin coat the part...
mrlindeman
-
10 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search