Davidpetty1988
Davidpetty1988
Supreme Being (298 reputation)Supreme Being (298 reputation)Supreme Being (298 reputation)Supreme Being (298 reputation)Supreme Being (298 reputation)Supreme Being (298 reputation)Supreme Being (298 reputation)Supreme Being (298 reputation)Supreme Being (298 reputation)
Group: Forum Members
Posts: 26, Visits: 89
I just made a 10 inch by 10 inch square as a test I made with a 2\2 twill 200g surface, 2 300g sandwich layers with weaves running a 45° angles I forget what that's called and finally another 200g for a backing layer, its light has a bit of flex and is very strong. . going to make a few tea cup coasters for the "beys" I feel bad not doing a thankyou to davro I'm a YouTube subscriber already watched pretty much all your cf videos your car is sick brahhh. I like that bonnet with the tow weave it looks proper narley. Thankyou warren and matt I have absolutely no doubt I'll be contacting you both for your valuable expertise in the field of composites I've got a lot of learning to do. 
THANKYOUUUU!!! EVERYONE!!!
David

P.s Peace out davro
http://www.talkcomposites.com/Uploads/Images/dc3fa9bb-432a-48ae-b13f-a8de.jpg
Edited 9 Years Ago by Davidpetty1988
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi David,

You're very welcomeSmile. It's a privillage to be able to do a job where we can do what we love, work with so many great customers and contribute to their enjoyment of these brilliant materials and processes.

I wish you every continued success but I'll warn you, there may be some heartache too one day - but we'll be there to help then too.

All the best, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Glad to hear your first project has gone well.

It really is quite satisfying to pull out that first part and even if it isn't perfect you can usually see how good it can be with a bit more practice.

Good luck with future projects and if you need any help correcting the defects for next time then ask away as there is a wealth of experience on this forum with resin infusion.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
davro
davro
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
Right on David

Edited 9 Years Ago by davro
Davidpetty1988
Davidpetty1988
Supreme Being (298 reputation)Supreme Being (298 reputation)Supreme Being (298 reputation)Supreme Being (298 reputation)Supreme Being (298 reputation)Supreme Being (298 reputation)Supreme Being (298 reputation)Supreme Being (298 reputation)Supreme Being (298 reputation)
Group: Forum Members
Posts: 26, Visits: 89
Just completed my first ever carbon fibre part at 2am and I'm so happy I had to tell someone!!!! It ain't perfect but for for a first time resin infusion I'm more than ecstatic with the results! Thank you so much everyone at ec for your awesome products customer service tech advice videos and sharing the knowledge. Thanks to everyone on this forum I've learnt alot from all the questions you all ask and learnt a lot from the mistakes that people made so I don't make them :-) 
THANKYOUUUUU!
keep on carboning!
Dave