Hi

I'm very new to all this so please be gentle!

I tried my first infusion mould at the weekend. After perserverence I seem to be struggling with leaks around the hose - bag seals.

However, what looks very simple in the online videos...ie putting the hose through the bag & into the silcone connector is always causing me leaks. I've tried tiny knicks in the bag to a bigger cut.

Should the hose force the bag in with it into the silcone connector?

What appears to happen is when the vacuum is applied wrinkles form around hose area & cause the leak.

Any help would be much appreciated on what appears to be quite simple.

Thanks in advance
Marcus
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search