one off plug/mould
one off plug/mould
Post Reply
Like
5
one off plug/mould
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
jaffa
jaffa
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 17,
Visits: 325
I want to make some one off ducts in Carbon, smooth on the inside for airflow. I've made a rough male plug and about to skin it and apply pattern coat primer.
My question, can I infuse straight onto this surface, then just remove the plug/mould from inside (ensuring there's no mechanical lock) or will the primer not tolerate the resin? Seems a waste of materials to make moulds as they'll be fairly big
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
one off plug/mould
jaffa
-
11 Years Ago
The primer would handle the resin fine, your issue will be crushing the plug. Don't underestimate...
Hanaldo
-
11 Years Ago
Another option is to make your plug longer on the ends than your part, essentially making flanges on...
nc42
-
11 Years Ago
Brake ducts are essentially a tube though, so it will always need envelope bagging unless you made a...
Hanaldo
-
11 Years Ago
[quote][b]Hanaldo (20/11/2015)[/b][hr]Brake ducts are essentially a tube though, so it will always...
jaffa
-
11 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search