Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Filling in small holes on carbon fibre part
Filling in small holes on carbon fibre part
Post Reply
Like
27
Filling in small holes on carbon fibre part
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Lenny
Lenny
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 16,
Visits: 58
After performing a resin infusion on my carbon engine cover am I left with a few holes in the surface. Is there a repair process to fill these in ? My thoughts are that I could mix some epoxy and hardener and simply fill in the holes and then sand/polish afterwards.
just wanted to check if there is anything special tips/tricks that could help.
Regards,
Lee
Reply
Like
27
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Filling in small holes on carbon fibre part
Lenny
-
11 Years Ago
Hi Lee Ifit's bare carbon, with no in-mould coating, then you'll find it impossible to flat and...
MarkMK
-
11 Years Ago
[quote][b]Lenny (18/11/2015)[/b][hr]After performing a resin infusion on my carbon engine cover am I...
fgayford
-
11 Years Ago
Both the techniques above will work fine. Whatever you do, the key is to make sure no dirt remains...
Warren (Staff)
-
11 Years Ago
Cheers guys, i will start the slow process of cleaning and sanding. Regards, Lee
Lenny
-
11 Years Ago
Post Reply
Like
27
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search