Group: Forum Members
Posts: 50,
Visits: 448
|
I just tried the product to one of my difficult mould and i was not able to get it sit over the mould properly. I should try to easier mould for first. I laid some carbonfiber with epoxy over the FlexPLAS and the flat part released extremely easy. It didn't stick at all. So releasing is extremely good. Now I just have to figure out will it be suitable for my moulds, or will it need a more even surfaces. If I put too much Flexplas, it will make wrinkles. if i put too less it will not stretch to all corners. At least they got good customer service. I must have a skype conversation with them and ask some more tips how to apply it. Very promising product for extremely easy release, but at the moment for me very difficult to apply properly. maybe i do something wrong.. lets see.
|