It is actually very difficult and incredibly easy all at the same time.
if you are good with your hands a quick to learn you will succeed, if not you will fail miserably!
watch the EC videos on making a bonnet and then make a honest decision, can you do as the video or not.
you cannot cut corners and need to follow the principles accurately, it can work, ive made parts for my bike so anyone can.
read,read and then read some more.
the uni-mould kit covers .7m so two should do a bonnet.
|