By djtd - 11/14/2015 11:25:56 PM

How much materials would I need to make a mould of my Audi A5 bonnet (hood)? I'm looking to make a carbon bonnet for it and it will be my first project. I have seen the kits on sites but I'm not sure on how much of what it is I would need. Any help will be appreciated. Anthony.
By jaffa - 11/18/2015 9:35:54 PM

i did a boot for my first attempt including infusion! So don't be shy, I would start with a smaller part first though to limit costs on the first few attempts that go in the bin Smile