Iam working on a MDF pattern. I still have some sanding to do on the MDF. When I am finish sanding it I am unshure on how to proceed. 

Should I apply pattern coat primer on each part before I glue the parts together?
How many coats of pattern coat primer does it looks like I will need? It should be quite straight when Iam finish with the sanding. 
I plan on applying a coat of hi gloss pattern coat before polish. 
Should I apply the pattern coats with brush or gun?

http://www.talkcomposites.com/Uploads/Images/a22774b4-24d0-423b-b1ae-edf8.jpg
MarkMK
MarkMK
Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
Difficult to see from the picture, but if gluing your two halves together will leave a join line that will form part of your mould then feels like you need to glue then paint the whole pattern in one go. 

Number of coats will depend on the finish you achieve on your first coat, but key between coats if you need to build up a decent thickness of coating to flat back. Spraying will give you a better finish but if the part's not overly large then working through the brush marks shouldn't be too bad. It's likely that you'll break through to the pattern surface at some points, so might be best to re-coat only when/if this happens.

 A foam pad or roller might give you a better finish, though, if spraying's not an option