20_rc51_00
20_rc51_00
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 95,
Visits: 548
I'm looking to pour foam into a cavity that has roughly the shape I need. Can I use PVA over the cavity surface so that I can pop the cured urethane out without destroying the cavity surfaces?
Reply
Like
3
Hanaldo
Hanaldo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Yep, works very well.
Reply
Like
3
20_rc51_00
20_rc51_00
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 95,
Visits: 548
Thanks!
Reply
Like
3
TURK
TURK
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 101,
Visits: 662
Can I just jump in OP ? ....... as what you're doing sounds like what I'm about to do.
Would you use mould release in the mould before the PVA ?
TURK
Reply
Like
3
20_rc51_00
20_rc51_00
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 95,
Visits: 548
I was just planning on coating the Cavity(mould) with PVA to keep things simple.
Reply
Like
4
Hanaldo
Hanaldo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
No need to use anything other than PVA.
Reply
Like
4
TURK
TURK
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 101,
Visits: 662
Lovely ..... thanks guys
TURK
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search