Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
A-stage and B-stage... huh?
A-stage and B-stage... huh?
Post Reply
Like
3
A-stage and B-stage... huh?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Joe
Joe
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 310,
Visits: 1.5K
Hey,
Searching the internet to learn a bit more about composites, I found that:
A-Stage and B-stage.
It seems to be related to resin used in prepregs... But i could not find any explanaition.
Anyone can help ?
 
 
    A $1000 electronic device will always protect a 10 cents fuse
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
A-stage and B-stage... huh?
Joe
-
13 Years Ago
Hi Joe, A-Stage: Not a term often encountered but this describes resin in the earliest stages...
Paul (Staff)
-
13 Years Ago
Thanks for the answer.
Joe
-
13 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search