Amateur from lancashire


Author
Message
Eeskidmark
Eeskidmark
Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)
Group: Forum Members
Posts: 6, Visits: 106
Hello All,

I am new to this forum and especially new to composites.

I have just finished Uni having done an engineering degree, so that is probably why I have the lust to try my hand at moulding carbon fiber parts.

I have got myself a couple of kits, the mould and an infusion kit.

Here is a couple of pictures of my first mould, its for an old British mx, a front mudguard brace. I hope to make the mudguard next. 

I filled all the small gaps up between the sign board with Plasticine although I feel filleting wax may be easier to use.  

http://www.talkcomposites.com/Uploads/Images/7dda758a-dbcc-43b7-8a2f-9f1a.JPG
http://www.talkcomposites.com/Uploads/Images/8622a4fe-543a-49db-a6e1-ca24.JPG


http://www.talkcomposites.com/Uploads/Images/89282194-f598-4f72-aeec-afeb.JPG
http://www.talkcomposites.com/Uploads/Images/e85df64b-ef48-4d51-b388-2abd.JPG


Please let me know if I have made any rookie mistakes. I am guessing that half the battle is managing to make a good mould.

How does carbon fiber hold up with cyclic fatigue such as heavy vibrations from the engine? should I be adding a reinforcement layer of kevlar?



One last quick question, I would like to create the part below for my other bike, but I dont want to make a cover for it I actually want to make it. Should I mould both sides then glue the two carbon fiber pieces together?

http://www.talkcomposites.com/Uploads/Images/d821aa0a-15c5-4252-a921-cb6f.JPG
http://www.talkcomposites.com/Uploads/Images/70cf8ee2-7511-43fd-80fc-463d.JPG




Cheers,

Henry





GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search