I think you should start looking for some PU resins (polyurethane) you can find them in different shores from soft to foamy to strong you should be able to find a rubbery texture. Or you could try latex. Best of luck Wink 

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




brendan
brendan
Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)
Group: Forum Members
Posts: 1, Visits: 2
Hallo
I am moulding some customised translucent push-buttons, and have previously used 2-part condensation cure silicone gel (from Tiranti). I would like a solution that produces buttons that are very soft and compressible, almost as soft as rubber foam; should I investigate silicone gel or epoxy resin?

Thanks
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search