Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Saul, have you tried warming it up a bit? I believe an issue with RTV silicones is they suck the heat out of the process, so thermoset resins may not reach the temperature they need to fully cure. If you warm everything up to about 30-40 degrees Celsius, you might find that solves the curing tacky issue.
|