ChrisR
ChrisR
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 363,
Visits: 3K
Anyone else had problems with pigmenting epoxy?
I added a gnats danglies worth of red epoxy pigment to a tester of the normal resin I use, 18hrs later and it's still not gone off properly, mix ratios were definitely correct, temperature has been reasonably consistent.
I've not pigmented epoxy before (poly yes, epoxy no) so does it retard the cure time?
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
pigment issues
ChrisR
-
11 Years Ago
No it certainly shouldn't... I've even added up to 10% by weight without any issues (though I...
Hanaldo
-
11 Years Ago
As honaldo said, it should be fine. I've mixed pigment up to about 10% before too and it's cured ok....
dbcrx
-
11 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search