Without some kind of drawing/image, this is very hard to suggest any approach to... My initial impression is that it will be very hard to do in a CF composite.

You are expecting it to handle a load of slightly above 10 kg perpendicular to the tube, without "bending"   = Not possible, it will bend, question is how much you can tolerate.
 With a wall thickness of 0.1 mm and a length of 35 mm ..

I could probably make such a tube from Beta-titanium --- I would not care to speculate on the price though ... CoolWhistling

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
edwardone333
edwardone333
Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)
Group: Forum Members
Posts: 1, Visits: 7
Looking for possibility to produce tube length 35 mm ,OD 2.7 mm ,ID 2.5 mm .
Ability to handle axial load up to 100 N without bending
Tapered end length is about 3 mm (could be adjusted) .Front hole is 2 mm diameter on tapered side
2 funneled side holes 4 mm away from tapered end
Can you please outline for me approach/area of composites that can meet these requirements
Cannot attach stl file 


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search