car splitter


Author
Message
spoonerboy1234
spoonerboy1234
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Awaiting Activation
Posts: 1, Visits: 8
hi im after some advice im wanting to make a splitter out of carbon iv already made a template out of mdf and sealed it with pva im not wanting the carbon to stick to the mdf so id be needing the laminating kit  iv downloaded the laminating guide but it the wrong way round for me  my finish surface will be last  what would the process be to made one

strenght wise what would i be needin

 iv looked at the carbon 2/2 twill 12k 650g as a base layer only 1 layer

and the 2/2 twill 3k 195g as the final layer same again 1 layer  would the be strong enough

looking at the kit iv worked out what i think id need is this correct

Carbon Fibre 2/2 Twill 3k 195g 1.25m Wide    £30.68     * *     £61.36    
Epoxy Laminating Resin 1kg SLOW    £16.75     * *     £16.75    
Professional Composites Snips    £8.27     * *     £8.27    
PVA Mould Release Agent 1litre    £6.55     * *     £6.55    
Mirka Waterproof Wet and Dry Combination Pack    £19.95     * *     £19.95    
Mirka P2000 Waterproof Wet and Dry Abrasive Sanding Paper 10 Sheets    £3.65     * *     £3.65    
Carbon Fibre 2/2 Twill 12k 650g 1m Wide    £25.00     * *     £50.00    
Epoxy Coating Resin 1kg Pack

many thanks chris
Edited 14 Years Ago by Matt (Staff)