Mouldphorm PCL Low-Melt Thermoplastic Moulding Granules is not suitable for making molds also in parts of the body like, hand, arm, shin?

Best Regards,
Jorge Ferreira
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
None of the traditional composites moulding materials will be suitable as they simply aren't safe to be in contact with skin. 

You would be looking towards medical grade plaster, silicone or alginate type materials and methods as they are designed for that purpose.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Pakito
Pakito
Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)
Group: Forum Members
Posts: 9, Visits: 33
To make body parts molds which will be the best way?
Plaster bandages coated glass fibers and epoxy resin or polyester?
Can make the mold with a polyester resin and then construct a laminate of carbon fibers with epoxy resin on top of the polyester resin mold?
For a cast of a hand, foot, arm, leg, the most advantageous option in terms of costs and time?