Yeah ... I did some electronics work, using glue lined shrink tube, and we had all kinds of problems with overheating other parts of the assembly with the heat gun. I then tried putting the assembly with the shrink tubing in place, into a curing oven and ramped up the temperature until I had a complete shrink down of the tubing .. that required the oven to ramp up to +120 degrees Celcius.. 

 Thats why I am a bit wary of using shrink tubing for making CF tubes...
 I've gone the other way and made up a "mandrel + outside compression mould" setup.  I found a local company that makes Nitrile rubber parts, they made some inflatable thick walled tubes for a friend, who wanted to produce a lot of composite tubes.  Fo my use I could not justify the cost of these tubes, so for some of my CF-tubes I used bicycle innertubes as internal compression.
I inflated the inner tube to hold the fabric and resin in place, then envelope bagged the whole setup and then vacuum on 

I made some "precision" tubes by first turning a tube mandrel to the desired outside diameter, then polishing it and making up a split mould from that. I then turned down a piece of the same Alu tube to the desired inside diameter and polished that .. I "cheated" a bit on the inside mandrel and made it very slightly tapered, about 1/10 of a mm over 50 cm length .. That makes releasing it a lot easier 
                
			            				
			            "Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)