Mirror cap for Ford Focus ST


Author
Message
tomzi1234
tomzi1234
Supreme Being (503 reputation)Supreme Being (503 reputation)Supreme Being (503 reputation)Supreme Being (503 reputation)Supreme Being (503 reputation)Supreme Being (503 reputation)Supreme Being (503 reputation)Supreme Being (503 reputation)Supreme Being (503 reputation)
Group: Forum Members
Posts: 40, Visits: 500
From first minute that i bought my car, i wanted to have carbon fibre mirrors.
So i start a project.
First i made split mould
http://www.talkcomposites.com/Uploads/Images/6419c48c-3ad1-4ffa-be90-8fc4.jpg
and than wet layup and vacuum-bag
http://www.talkcomposites.com/Uploads/Images/f9e308a8-7e4a-4ea7-befa-99bd.jpg

after quick edges trim, test if if fits.
http://www.talkcomposites.com/Uploads/Images/78943a36-5511-4d7e-965b-39f3.jpg

Than some sending and resin layer and more sending and polishing.
But i think it turned out great Smile
http://www.talkcomposites.com/Uploads/Images/68a2c6c8-b259-496b-aa5f-360f.jpg

Now the second one is waiting to be layed in mould.