After several test panels I have gone with framing the outside of the panel with end grain balsa to allow for fixings with Aluminum hex core
With weight, stiffness and impact resistance all being important I am toying with the idea of using a double sandwich as my 2.5 mm build up in Kevlar and Diolen feels to flexible as an outside layer
Any suggestions for this, I'm thinking 2 layers kevlar both sides on a 2.5mm coremat as the outer shell then the hexcore etc
|