Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Pattern and Plug Making
»
Mold sharp edges?
Mold sharp edges?
Post Reply
Like
3
1
2
Next
Jump To Page
Mold sharp edges?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
TomDesign
TomDesign
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
Guys what is used here from these guys for sharp egdes? they use same method for bodykit stuff also for the corners?
Thank you in advance
Reply
Like
3
George Sychrovsky
George Sychrovsky
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 24,
Visits: 1.6K
Usually a mix of flox and silica
---------------------------------------------------------------------
Disclaimer opinions of others will vary depending on what they are selling
Reply
Like
3
TomDesign
TomDesign
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
what is that? any link?
Reply
Like
2
Matthieu Libeert
Matthieu Libeert
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
here are some links
with materials to thicken your resin
http://easycomposites.co.uk/products/resin-gel-silicone/fillers-and-additives/aluminium-tryhydroxide-filler-powder-for-casting-resins.aspx
http://easycomposites.co.uk/products/resin-gel-silicone/fillers-and-additives/glass-bubbles-microballoons-microspheres.aspx
http://easycomposites.co.uk/products/resin-gel-silicone/fillers-and-additives/fumed-silica-thixotropic-powder.aspx
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
TomDesign
TomDesign
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
Matt any info how much those things put into resin?
Reply
Like
3
Matthieu Libeert
Matthieu Libeert
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
cant tell... but it can take quit a lot, depends on how thick you want it and for how much resin.
used it 50/50 in volume at some time...look for cotton flakes as well got a box of the brand west systems laying around somewhere, worked well
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
TheCompositeLab
TheCompositeLab
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 1,
Visits: 4
You have to be careful about using fillers like that on sharp mould edges, you are better off using roving and really getting it into the corner. Fillers tend to chip out with repeated use of the mould. You want to keep fibers against your gel coat, not filler.
Reply
Like
2
TomDesign
TomDesign
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
so what you suggest to use any image or link on sharp edges for molds or pieces from mold.? Guy suggested silica to use?
Reply
Like
3
Hanaldo
Hanaldo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Better to use loose chop strand. So the same stuff that makes up chop strand mat, but not bound together. Like so:
Mix it in to your resin handful by handful until it is a consistency that suits what you need.
Reply
Like
2
VVS
VVS
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Moderators
Posts: 226,
Visits: 334
That's a great little tip.
most people are throwing small off cuts away but chopping them up then saving them in a bag till such a time is a great idea.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
1
2
Next
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search