Hello,

I am trying to determine both the young's modulus and shear modulus of the PVC closed cell 25mm thick foam core. Has anyone done some tests and can help me out? Finding it very hard to get an accurate G value.




Thank you,




Hannah
Warren (Staff)
Warren (Staff)
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
I have attached the Technical Data Sheet with the mechanical properties. Hopefully that should help you calculate the information you need.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Attachments
EASYCell-40-75.pdf (1.6K views, 41.00 KB)