Carbon Fiber Intake Tube


Author
Message
mitchedwards
mitchedwards
Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)
Group: Forum Members
Posts: 2, Visits: 9
Hi guys I'm new here and new to making my own composites! I am a third year Mechanical Engineering student in Canada.  What I want to do is make some carbon fiber parts for my truck which include; Intake tube, Turbocharger tube, and Intercooler tubes to start.

I have began making my intake tube plug utilizing the following materials:
Foam - Floracraft Dry Foam from michaels craft store
Basic hot glue
Bondo Gold body filler
Filler primer
Duplicolor engine paint

I just received my prepreg carbon fiber from Composites Canada (196gsm and 670gsm) and I attached the spec sheet they sent me.

My plan was to make the mold from the prepreg as it will cost me the same as to do  a wet layup fiberglass mold vs prepreg.

Do I need a gelcoat for a prepreg tooling mold?

My vacuum pump will only get about 17 inhg at sea level, will this be sufficient?

Will my plug hold up to curing the mold in an oven? I will need to make an oven, any suggestions?

Sorry about all the questions guys I have spent about 2 months researching and am getting really excited!

The pictures are of my plug installed in my truck to verify fitment.

Thanks guys!

Attachments
IMG_0725.JPG (594 views, 1.00 MB)
IMG_0727.JPG (558 views, 1.00 MB)
Hexply Carbon Fiber M35_4_eu.pdf (645 views, 350.00 KB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search