VVS
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Moderators
Posts: 226,
Visits: 334
cheers
i have a few panels im working on and although the paint is good im pretty sure its from spray cans.
i took a mould off the front mudguard and paint came off and stuck to the gel coat so i will re work the rest with a 2k coating.
Reply
Like
3
Matthieu Libeert
Matthieu Libeert
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
A Two component (2K) is the best... base + hardener
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
2
VVS
VVS
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Moderators
Posts: 226,
Visits: 334
Reading that rattle cans are a no no when using oe bike panels for patterns.
what is the best paint type to spray them with.
I have access to paint facilities so can spay most any type.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search