Group: Forum Members
Posts: 7,
Visits: 67
|
Hi Tom,
Thanks for your reply. That's good news that we can use standard gelcoat, however, I'm a bit concerned about how thick the gelcoat is as the carbon weave texture is visible, I would imagine to get a 7.5m boat including ama to weight 9.8kg, it will be thin. Also, how easy is it to match the colour?
I have also noticed, since posting, that the colour sections on the top deck seem to be applied vinyl sections as their edges are raised as opposed to being under the gelcoat, I am waiting for a response to the manufacturer as to what these are but if they are applied vinyl sections and the bubbling in this area is in the gelcoat under them, this will complicate things.
We are in Stoke-on-Trent, so within easy traveling distance of Nottingham. When you say you may be able to help, do you mean in assessing it further or do you do repairs?
|