Hi

I hope you can help me ,I am looking for something to coat my fishing lures. It needs to be really hard and  able to resist scratches from the hooks . With lures costing so much these days they put on a cheap coating that does not last very long. All lures to be coated are plastic.

Kind Regards Gary
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The hardest resin we have for such an application would be our Epoxy Coating Resin

Once cured, it is waterproof and will have a hard finish.  It will eventually scratch, no resin is scratchproof, but can be sanded smooth and repolished if needs be.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search