My Vac pump is a small laboratory unit (oil filled)  It is built to run continously for as long as needed, and uses only around 100W  so I just leave it on until the stack has cured.

It has a return valve to prevent the oil being sucked back out of the pump.  (Seems a simple precaution, but not standard on the EC pump??)
 

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
JustJDee
JustJDee
Supreme Being (193 reputation)Supreme Being (193 reputation)Supreme Being (193 reputation)Supreme Being (193 reputation)Supreme Being (193 reputation)Supreme Being (193 reputation)Supreme Being (193 reputation)Supreme Being (193 reputation)Supreme Being (193 reputation)
Group: Forum Members
Posts: 13, Visits: 153
Ohh sorry, didn't see that cause of the photo!

Thanks mate Smile
JRT
JRT
Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)
Group: Forum Members
Posts: 13, Visits: 130
Question... while the vaccum parts are curing on a oven should the pump be working during the all 8h of curing?
Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
JRT (18/02/2015)
Question... while the vaccum parts are curing on a oven should the pump be working during the all 8h of curing?


If you have a perfect vacuum there should be no need to lkeep it running 

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




JRT
JRT
Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)
Group: Forum Members
Posts: 13, Visits: 130
I thought so, thanks for the quick reply.
Pakito
Pakito
Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)
Group: Forum Members
Posts: 9, Visits: 33
Epoxy resin can be crafted in a vacuum?
What curing time for a piece of carbon fiber with epoxy resin?
A part cured in a vacuum is the same effect as in the oven?