Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Yes it will work on a dry painted floor. Ideally give the floor a light key and ensure the floor is free of dirt and dust to maximise adhesion.
We would recommend you test a small area first to ensure the paint itself is not damaged as some paints will be damaged under the resin.