Hi,
I am planning on making larger moulds(car panels etc) and hoping to do so using the Uni-Mould system, my only reservation is the MEKP Catalyst. As I am from Ireland I cannot get you guys to ship it and I have never heard of anywhere that would supply it.

So my question is what kind of place might supply the catalyst, would an Auto paint specialist stock it?
Or is there an alternative

Thanks in advance
Edited 10 Years Ago by Pconn061
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
I believe it is different reactivity levels but you are best checking with the manufacturer to be sure.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Miguel0885
M
Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)
Group: Forum Members
Posts: 3, Visits: 3
Warren (Staff) - 12/7/2017 9:21:29 AM
I believe it is different reactivity levels but you are best checking with the manufacturer to be sure.

Thanks for the reply. I will try to contact them.

How about Cenox M50? Is that something similar as what you sell?

Here is a link of what I found
https://shop.swiss-composite.ch/pi/Harze/Polyester-UP/Additive/MEKP-Haerter-M20-M50-M60.html?von_suchresultat=true

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Pconn061 - 10 Years Ago
Warren (Staff) - 10 Years Ago
Miguel0885 - 8 Years Ago
Brian_s - 10 Years Ago
Ian Mantula - 10 Years Ago
Hanaldo - 10 Years Ago
Warren (Staff) - 10 Years Ago
Ian Mantula - 10 Years Ago
Hanaldo - 10 Years Ago
Hanaldo - 10 Years Ago
ajb100 - 10 Years Ago
Warren (Staff) - 8 Years Ago
Miguel0885 - 8 Years Ago
Warren (Staff) - 8 Years Ago
Miguel0885 - 8 Years Ago
Warren (Staff) - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search