my hubby (novice at this) is trying to make acrylic blanks from clear casting resin to make pens. so far his attempts (not good). they have been very hard and brittle not good for turning on lathe. Can you suggest for 2 ozs of resin, how much catalyst to use
and does adding liquid colour make a difference to hardness. hears hoping for an answer!