Catch can only needs to be as big as the amount of resin you plan to let in it. You don't necessarily need a catch can at all, it's only job is to catch any resin that gets evacuated from your part before it destroys your pump. I myself have a 1L catch can, and it's never had a drop of anything in it. 
AHA
AHA
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 6, Visits: 14
Hi what catch pot size would I need to make a  carbon bamboo sun lounger? Would I be right in thinking the bigger the part being manufactured the bigger catchpot required ? 