Help with Mould Design!


Author
Message
baja_patient
baja_patient
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 135, Visits: 1.6K
Hello Guys!

Have been off the scene for a while, but I feel a project coming up very shortly. Have been flying a lot of model aircraft lately and have a beauty of a waterplane. The thing is it came with some very very light glass fiber floats, I assume about two layers max. of some light cloth. Some harder landings cause them to crack in sum places and flex causing paint to chip off. I would like to produce them in Carbon Fiber, (2 layers light cloth 90 or 130 g per sqm) in infusion, possibly with inmould coating/gel coat.

My initial questions to everybody out there now are, what would be the best way to go about making these moulds, ideally I would make a two part (seperate, not split) vertically down the center line, so the parts could be subsequently joined.

The pictures show the potential plug I will be using.

http://www.talkcomposites.com/Uploads/Images/f1075238-00a6-4730-b906-d43b.JPGhttp://www.talkcomposites.com/Uploads/Images/5205788a-2dd5-4f10-86b8-1cab.JPG
http://www.talkcomposites.com/Uploads/Images/28b1fbfc-a82f-4e1b-b168-9755.JPG
 
http://www.talkcomposites.com/Uploads/Images/70ec63b1-f6e3-4f73-b9f3-3e60.JPG

http://www.talkcomposites.com/Uploads/Images/f5de71e3-459b-4426-89f0-53a9.JPGhttp://www.talkcomposites.com/Uploads/Images/d079d349-d39f-4704-8e81-6c62.JPG

I would make two moulds (halves) for one float, because they are symetric, apart from the tabs, which can be subsequently installed in a mirrored fashion.

I would be willing to cut a float lengthways if needed. Was planning to try the unimould system.

All ideas are welcome! Lets hear them!

Cheers