Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
UD Prepreg
UD Prepreg
Post Reply
Like
6
UD Prepreg
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Chrisa
Chrisa
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 10
Do you or can you supply UD prepreg and if so what variety of cloth is available? If not do you know if it may be available from other suppliers?
I already use your UD for carbon road frame fabrication but wanted to begin curing at higher temperature to increase performance (reduce weight/ increase stiffness).
If my options are limited to infusing the cloth myself, which resin do you suggest for curing at 80 - 100 oC?
Many thanks.
Reply
Like
6
Warren (Staff)
Warren (Staff)
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Unfortunately we do not currently stock a UD carbon pre-preg material.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
6
Trace Elliott
Trace Elliott
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 4,
Visits: 30
Hi,
It's too bad you don't offer UD prepreg, it limits the possibilities when making complex parts.
Do you have any plans to stock UD prepreg in the future? If not, why?
Would it be a problem to mix Vari-preg with a UD prepreg from a different resin system ?
Thanks!
Reply
Like
6
Warren (Staff)
Warren (Staff)
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
We are currently working on expanding our range of pre-pregs later this year so it may be something we consider then.
We haven't had a UD pre-preg up until now as there hasn't been significant enough demand to make it financially viable to stock the large quantities we would need to get a good retail price and sell it within it's expiry date.
In terms of mixing different pre-preg types, without testing it would be impossible to say for sure if the materials would cure properly with a high quality inter-laminar bond strength.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search