Hi

I was wondering if it was possible to dissolve the PU 80 low density model board in some solvents after having laminated a CF cloth around it ?

The idea would be to
- cut the foam to the target shape
- apply the epoxy/CF cloth
- dip the hole thing in a jar of acetone / other solvent



Thanks for your help !
P.
Replies
baja_patient
baja_patient
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 135, Visits: 1.6K
Hi, I'd like to apologize for the false information. I got my foams mixed up. I built a surfboard once and regular styrofoam and high density closed pore foam were non compatible with polyester. 

As for the acetone, I poured it into a regular plastic drinking cup, the cheap throw-away kind which I assume is PVC, and the bottom just fell out instantly. I was using class A acetone, which I bought from an epoxy supplier specially to clean epoxy tools. 

As for dissolving the cured epoxy, I had a strong hunch that its chemical proof-to resistant when fully cured. It did however come to mind that in your uni-mould video, the first one, you use acetone in a spray bottle to tack the cloth to the cured resin. Then I remembered it was polyester. 

Anyways I am obviously by no means an expert and am learning everything I can. I now know more and will thus shut up for a while! BigGrin

Good luck with the project. 

Cheers
steveastroUK
steveastroUK
Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)
Group: Forum Members
Posts: 21, Visits: 78
[quote][b]baja_patient (30/04/2012)As for the acetone, I poured it into a regular plastic drinking cup, the cheap throw-away kind which I assume is PVC, and the bottom just fell out instantly. I was using class A acetone, which I bought from an epoxy supplier specially to clean epoxy tools. 
/quote]

Usually polySTYRENE, NOT PVC - which is as much of a sod to dissolve as PU.

Steve
baja_patient
baja_patient
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 135, Visits: 1.6K
steveastroUK (05/05/2012)
[quote][b]baja_patient (30/04/2012)As for the acetone, I poured it into a regular plastic drinking cup, the cheap throw-away kind which I assume is PVC, and the bottom just fell out instantly. I was using class A acetone, which I bought from an epoxy supplier specially to clean epoxy tools. 
/quote]

Usually polySTYRENE, NOT PVC - which is as much of a sod to dissolve as PU.

Steve




Hmm yeah probably, but the cup was clear. Didnt know you could get clear polystyrene cups. not the white coffee ones. 

Nevermind, I use glass now and no solvent will dissolve that. 
steveastroUK
steveastroUK
Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)Supreme Being (211 reputation)
Group: Forum Members
Posts: 21, Visits: 78
Yeah, polystyrenes come in clear as well as expanded forms.
Pertabolis
Pertabolis
Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)
Group: Forum Members
Posts: 17, Visits: 193
baja_patient (06/05/2012)

Nevermind, I use glass now and no solvent will dissolve that.







Unless yo are using fluoridric acid !BigGrin
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Pertabolis - 13 Years Ago
baja_patient - 13 Years Ago
Pertabolis - 13 Years Ago
baja_patient - 13 Years Ago
Pertabolis - 13 Years Ago
baja_patient - 13 Years Ago
Matt (Staff) - 13 Years Ago
baja_patient - 13 Years Ago
steveastroUK - 13 Years Ago
baja_patient - 13 Years Ago
                     Yeah, polystyrenes come in clear as well as expanded forms.
steveastroUK - 13 Years Ago
Pertabolis - 13 Years Ago
Pertabolis - 13 Years Ago
Matt (Staff) - 13 Years Ago
Pertabolis - 13 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search