Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
The base resin in all our polyester pigments is polyester resin itself so it should not cause any curing issues and as the grey pigment has cured that would lead me to believe maybe you have been sent the wrong pigment.
If you would like to ring one of our team or email us with your order number and details we will happily try and sort it out for you.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|