Priming and finish coat for plug?


Author
Message
WHY69
WHY69
Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)
Group: Forum Members
Posts: 3, Visits: 30
I'm making a plug with polyurethane casting resin via silicone mould. I'm planning to then use this plug to make a mould from using the unimold system or similar product (for out of autoclave pre preg CF). I have plenty of questions but mainly I'm wondering if I should prime and gel coat the polyurethane casting resin (plug) prior to making the mould?  If so what products are compatible for what my plans are. 

Polyurethane casting resin plug>
Vinylester tooling coat etc mold (unimold)>
Prepreg carbon fiber out of autoclave finished product. 

I've read and read everything I can but I'm still unsure of what products will interact badly with others and I want to make sure if I need a primer and gloss coat for the mold I use something that will work. Obviously there will be a release agent between the plug and mold made from it but I don't want to use the wrong product that may react badly with the polyurethane casting resin. 

Thank you for any insight you folks might have. 
GO