Depends a lot on what material you are using, fabric density, mould size etc. I have successfully infused 10 layers of 663g twill weave carbon fibre before, but had issues with infusing 7 layers of 450gsm uni. So the easiest way to answer is for you to tell us exactly what you are wanting to make etc. 
kalyaniwe
kalyaniwe
Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)
Group: Forum Members
Posts: 2, Visits: 4
hai all,

 i am planning to make composite using vaccum infusion method...
 
 is the no of fabric layers are restricted... and what is the maximum no of fabric layers  for Infusion method..

 and what should be the vaccum level.