Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)
Group: Administrators
Posts: 134, Visits: 614
Hi Rod,

We don't sell anything, however, the EPDM draught-excluder seals that are available from most hardware stores are perfect, these have been used in many industrial vacuum press applications for years, they're self adhesive, hold a perfect vacuum and are cheap! here's a link to the sort of thing that I mean, i'm sure you'll be able to track some down locally.

EPDM Weather Strip Link

 

Paul Statham
Easy Composites / Carbon Mods - Technical
Rod Nelson
Rod Nelson
Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)
Group: Forum Members
Posts: 1, Visits: 3
Does the company supply O-section (or some other suitable) gasket extrusion for forming a vacuum seal between a rectangular frame-supported membrane and a flat surface?
I want to make a very simple vacuum press for repeat vacuum pressing of large flat areas, but need a very good seal.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search