Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - Product Specific Pages
»
Carbon Fibre Sheet
»
Is carbon sheet at all flexible?
Is carbon sheet at all flexible?
Post Reply
Like
9
Is carbon sheet at all flexible?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
BogBeast
BogBeast
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2,
Visits: 9
Hi Matt,
Thanks for your reply.
That helps very much, I will be buying some soon!
Paul
Reply
Like
10
Matt (Staff)
Matt (Staff)
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 680,
Visits: 1.9K
Hi,
All thicknesses of carbon fibre sheet will have a degree of 'bendability', the main influence being the thickness. If you went with a 1mm wet-lay sheet you would find it very easy to bend round the size of radious that you'll find inside a wheel arch but if you went up to a 3mm pre-preg then you'd find it almost impossible to bend at all.
If this is just a structural exercise (i.e. not cosmetic) and you really want to add some sturdy protection to the inside of the fenders then how about laminating some
175g kevlar cloth
with
epoxy resin
. It would be quick and easy to do and would have incredible resistance to wear; far better than carbon fibre sheet would. Also, you would have no concerns over it fitting around the contour - the dry material would be easy to laminate around any shape.
I hope this helps.
Best regards, Matt
Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Tags
abrasion
carbon fibre
kevlar
repair
sheet
Edited
14 Years Ago by
Matt (Staff)
Reply
Like
11
BogBeast
BogBeast
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 9
Hi
The front tyres of my kit car are fouling slightly on the GRP on full lock. It will gradually wear a hole I expect, so I want to fend it off.
There is a bit of a curve where is is rubbing, is this sheet at all flexible? I would like to try fix it over he area but but worry that this won't bend at all...
Thanks
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search