A method I use a lot for parts with open ends is expanding foam. Squirt some in each end, once cured trim/ sand to shape. Cover the foam in flash breaker tape or parcel tape and use filleting wax to fill the join line. Easy to work with and more substantial than card.
One thing to keep in mind with trim parts is that they often "relax" once removed from the car. You spend ages making a mould, then a nice shiny part to find that it actually no longer quite fits. The same is true when adding flanges, it is easy to change the shape or twist things slightly.
Warren

Carbon Copies Ltd
Edited 11 Years Ago by wozza
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Sometimes its simpler to just use thin card that will bend to shape, then cover with flash breaker tape. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
aza993a
aza993a
Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)
Group: Forum Members
Posts: 10, Visits: 91
Had much trouble with curved flanges. Now I like to use a cheap poster board for flange material, conforms to complex curves easily. I get the stuff that's got a slick polymer finish on one side that's non stick (the regular board I find is too flimsy), then brush a pva on it and tape overlaps.  For fillet, I use, I think it's drywall patch comes in a gallon container and fill zip lock bags, cut a corner out, then squeeze, let dry then pva.  Oh and use hot melt gun to stick the flange to underside of part. The flange does not have to be very stiff, just stiff enough to hold up to firm brush strokes.  Saves time, no cutting or transfering of shapes, just cut strips and go.

You could even do the layup directly on the part and add the flange secondary. 
Edited 11 Years Ago by aza993a
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Have a look at what I posted in here: http://www.talkcomposites.com/12113/Need-advice-on-how-to-flange-this?Keywords=Flanging#bm12129



You can get a much nicer radius than I did on the edges if you're using the yellow filleting wax, just use a pop stick and it comes out close to perfect. But doing it piece by piece is quite easy, doesn't take as long as you would expect.
whitecel
whitecel
Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)
Group: Forum Members
Posts: 19, Visits: 39
Hey guys,
  This may seem simple, but I've been baffled and frustrated in how I should tackle the ends of my door sill.  Short of using an enormous amount of fillet wax, how should I go about flinging the ends?  These are the two ends.  The only way I see it working is if I slowly cut and glue little by little to go around the curved edges.  Any help would be greatly appreciated.

Thanks in advance.

One side 


Other side












GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search