Hi I would like to cast components using 3D printed molds. The 3D printing process uses laser sintered nylon which has a rough porous surface, the first attempt using blue PVA release agent and polyurathane casting failed, and using Easy-Lease did not work well either with the casting material sticking to the mold. Do you have any recommendations on types of surface preparation, release and casting compounds ? Alternatively I could cast a silicon mold from a 3D printed positive, however dimensional stability is important - I am looking for 0.3mm in 100mm. Many thanks. Regards Paul
|