Here is my own design of swing arm cover and combined hugger for my little Aprilia RS250 project bike.. Hop you guys like it..



Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Good job! looks great!

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




pahanes
pahanes
Supreme Being (479 reputation)Supreme Being (479 reputation)Supreme Being (479 reputation)Supreme Being (479 reputation)Supreme Being (479 reputation)Supreme Being (479 reputation)Supreme Being (479 reputation)Supreme Being (479 reputation)Supreme Being (479 reputation)
Group: Forum Members
Posts: 29, Visits: 20K
Not bad ! 
Visible problems with varnish. I would have handled an abrasive and covered again.
davro
davro
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
morepower
morepower
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
pahanes (20/09/2014)
Not bad ! 
Visible problems with varnish. I would have handled an abrasive and covered again.


I did go over it again... The mould had a little damage so it needed several coats of lacquer.. 
morepower
morepower
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
I made a new mould to get rid of the small amount of damage and the step in the split line. The mould was made by a friend and it was OK but the halves were not interlocked so it could move. Now it can't... 

The customer wanted a matte finish so this one is his.


wozza
wozza
Supreme Being (8.5K reputation)Supreme Being (8.5K reputation)Supreme Being (8.5K reputation)Supreme Being (8.5K reputation)Supreme Being (8.5K reputation)Supreme Being (8.5K reputation)Supreme Being (8.5K reputation)Supreme Being (8.5K reputation)Supreme Being (8.5K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
NiceSmile Out of the mould finish or matt clearcoat?

Carbon Copies Ltd
morepower
morepower
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
That is a matt clear coat..... 
THE FLUTE
THE FLUTE
Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)
Group: Forum Members
Posts: 1, Visits: 45
That looks lovely Really like that.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search