Carbon bike frame repair.
Carbon bike frame repair.
Post Reply
Like
3
Carbon bike frame repair.
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Colin
Colin
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 6
I have a carbon bike frame and the down tube has a hole about 1" long (in direction of the tube) by 1/4"wide. Would your Carbon Fibre Rapid Repair Kit fix it? Also would a wrap of Lightweight Kevlar flat braid increase the strength of the repair? If it increases the strength, would you put this on first and then cover it with the repair kit treatment?
Reply
Like
3
Fasta
Fasta
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
Colin (22/08/2014)
I have a carbon bike frame and the down tube has a hole about 1" long (in direction of the tube) by 1/4"wide. Would your Carbon Fibre Rapid Repair Kit fix it? Also would a wrap of Lightweight Kevlar flat braid increase the strength of the repair? If it increases the strength, would you put this on first and then cover it with the repair kit treatment?
Don't worry about any Kevlar, all carbon will be stronger and easier.
Fastacraft Facebook page
Reply
Like
3
sebgron
sebgron
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 13,
Visits: 27
Have a look at this, although I would not recommend fixing a carbon frame unless you know exactly what you are doing.
Carbon Fiber Bike Repair- Video Tutorial 1 of 2
Reply
Like
2
Matthieu Libeert
Matthieu Libeert
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
I did a repair as well on a bike and made a tutorial on it.
https://www.youtube.com/watch?v=RQuy2D315Hk
Have a look, like stated above, be sure you know what you are doing and keep in mind it is still a risk you are taking to repair a broken bike frame
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search