Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
how to seal cardboard ?
how to seal cardboard ?
Post Reply
Like
3
how to seal cardboard ?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
palace
palace
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 6,
Visits: 41
I have a surface made of cardboard, that I need to take a mould
(rtv silicone)
from.
The cardboard have a lot of fine details, creases, cuts and scratches etc that I want to capture.
Any recommendations on how to seal (prepare the surface of) the cardboard before pouring the silicone..?
Edited
11 Years Ago by
palace
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
how to seal cardboard ?
palace
-
11 Years Ago
not sure but have you thought about using PVA? seen it a lot on cosplay posts and so on
matthieutje65
-
11 Years Ago
Thank you, I will look into it. What is the best way to apply it? I have a spray gun that I can...
palace
-
11 Years Ago
can be done with a brush or spray...have it laying around here at home but never used it :D sure...
matthieutje65
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search